Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 16.06 GPa | 2329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP SFL2A PA 12 (Asia Pacific) LNP* LUBRICOMP* SFL2A is a compound based on Nylon 12 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 16.06 GPa | 2329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP SFL2A PA12 LNP* LUBRICOMP* SFL2A is a compound based on Nylon 12 resin containing 50% Glass Fiber, 10% PTFE. Added feature of this material is: Wear Resistant. |