Mechanical Properties Metric English Comments
Tensile Modulus 10.96 GPa
1590 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EF006E PEI
LNP THERMOCOMP* EF006E is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.