Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.63 GPa | 1542 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL16 PA 66 LNP* LUBRICOMP* RFL16 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant. |