Mechanical Properties Metric English Comments
Tensile Modulus 10.53 GPa
1527 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM XH2315 TPI Resin
Extem XH2315 Resin
Tensile Modulus 10.53 GPa
1527 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Asia Pacific)
Extem XH2315 Resin
Tensile Modulus 10.53 GPa
1527 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Europe-Africa-Middle East)
Extem XH2315 Resin
Tensile Modulus 10.53 GPa
1527 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP KONDUIT PX10322 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compound, with through-plane and in-plane thermal conductivity of 1.7 W/(m*K) and 4.7 W/(m*K) respectively, conforming to ASTM E 1461 test standard.