Tensile Modulus 15.83 GPa
2296 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON WEF42I PBT
LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive.