Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.25 GPa | 1487 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East) VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors. |
|||
Tensile Modulus | 10.25 GPa | 1487 ksi | ISO 527 |
Azoty Tarnow™ TARNOFORM 500 GF6 POM 30% glass fiber reinforced, high flow injection molding grade, suitable for applications where high strength and stiffness is required, combined with higher flowability during molding.Information pr.. |