Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.009 GPa | 146.4 ksi | 50mm/min; ASTM D638 |
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade ALATHON M6080 is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include case.. |