Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 145 GPa | 21000 ksi | |
PSM Industries Pacific Sintered Metals Iron F-241-T Powdered Metal Low stressed mechanical components, Soft magnetic applications Equivalent MPIF Specification: F-0000-20Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Modulus | 145 GPa | 21100 ksi | |
Hexcel® HexPly® EH04 Epoxy Resin System, IM4 Fiber IM4 120 24" EH04 31%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel |
|||
Tensile Modulus | 145 GPa | 21000 ksi | 0°, Dry |
Hexcel® HexPly® 8551-7 Epoxy Matrix, AS4 Fiber Information provided by HexCel |