Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 95.1 GPa | 13800 ksi | |
PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-SH Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Information Provided by Pacific Sintered Metals, a division of PSM Industries |