Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.075 GPa | 1316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP KONDUIT MT00E PP LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing 70% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Tensile Modulus | 9.073 GPa | 1316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Asia Pacific) LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Tensile Modulus | 9.073 GPa | 1316 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Europe-Africa-Middle East) LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |