Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 1304 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 8.992 GPa

@Temperature 30.0 °C
1304 ksi

@Temperature 86.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..