Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.98 GPa | 2028 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6 LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity. |
|||
Tensile Modulus | 13.98 GPa | 2028 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6 4.0 specific gravity, Nylon 6 |