Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.56 GPa | 1967 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP UF006S PPA LNP THERMOCOMP* UF006S is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 13.56 GPa | 1967 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP UF006S PPA (Asia Pacific) LNP THERMOCOMP* UF006S is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |