Mechanical Properties Metric English Comments
Tensile Modulus 0.0900 GPa
13.1 ksi
1 mm/min; ASTM D638
ICO Polymers ICOFLOâ„¢ 510-5020 400 Micron LDPE Powder
Description: ICOFLO 510-5020 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Tensile Modulus 0.0900 GPa
13.1 ksi
1 mm/min; ASTM D638
ICO Polymers ICOFLOâ„¢ 510-5023 400 Micron LDPE Powder
Description: ICOFLO 510-5023 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Tensile Modulus 0.0900 GPa
13.1 ksi
1 mm/min; ASTM D638
ICO Polymers ICOFLOâ„¢ 510-5056 500 Micron LDPE Powder
Description: ICOFLO 510-5056 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Tensile Modulus 0.0900 GPa
13.1 ksi
1 mm/min; ASTM D638
ICO Polymers ICOFLOâ„¢ 510-5057 80 Micron LDPE Powder
Description: ICOFLO 510-5057 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Tensile Modulus 0.0900 GPa
13.1 ksi
1 mm/min; ASTM D638
ICO Polymers ICOFLOâ„¢ 510-5058 1200 Micron LDPE Powder
Description: ICOFLO 510-5058 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Tensile Modulus 0.0900 GPa
13.1 ksi
1 mm/min; ASTM D638
ICO Polymers ICOFLOâ„¢ 510-5062 500 Micron LDPE Powder
Description: ICOFLO 510-5062 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Tensile Modulus 0.0900 GPa
13.1 ksi
1 mm/min; ASTM D638
ICO Polymers ICOFLOâ„¢ 510-5063 800 Micron LDPE Powder
Description: ICOFLO 510-5063 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Tensile Modulus 0.0900 GPa
13.1 ksi
1 mm/min; ASTM D638
ICO Polymers ICOFLOâ„¢ 510-5064 1200 Micron LDPE Powder
Description: ICOFLO 510-5064 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Tensile Modulus 0.0900 GPa
13.1 ksi
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur..
Tensile Modulus >= 0.0900 GPa
>= 13.1 ksi
perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T92.100 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Tensile Modulus 0.0900 GPa
13.1 ksi
average; in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable..
Tensile Modulus >= 0.0900 GPa
>= 13.1 ksi
in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..
Tensile Modulus 0.0900 GPa
13.1 ksi
average; perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..