Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.931 GPa | 1875.5 ksi | ASTM D-638 |
PlastiComp Complet® LGF40 - PA6 Nylon 6, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |