Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0890 GPa | 12.9 ksi | 1 mm/min |
Arkema Group Pebax® MV 1074 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....) Permanent antista.. |