Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.85 GPa | 1864 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF008ESZ PA 66 LNP* THERMOCOMP* RF008ESZ is a compound based on Nylon 6/6 containing 40% Glass Fiber. Added features of this grade include: Easy Molding, Heat Stabilized. |