Mechanical Properties Metric English Comments
Tensile Modulus 12.84 GPa
1862 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66
LNP* THERMOCOMP* RF0069SZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of th is grade include: Flame Retardant, Heat Stabilized.