Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.58 GPa | 1825 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RX10408H PA 66 LNP* Thermocomp* RX10408H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare. |