Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0827 GPa | 12.0 ksi | ASTM Data |
Dow Prevail® 3050 ABS + Polyurethane PREVAIL® 3050 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |