Polymer Property : Tensile Modulus = 1142 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 7.874 GPa
1142 ksi
Storage
Epoxy Technology EPO-TEK® N20E Electrically Conductive Paste
Product Description: EPO-TEK® N20E is a two component, electrically and thermally conductive, epoxy adhesive designed for semiconductor and electronics assembly. Its applications and field conditi..