Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 76.19 GPa | 11050 ksi | |
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Fabric Form Material Description: F3G584-60; Fiber: T300-3K; T300/13.5 mils (0.343 mm) per plyInformation provided by HexCel |