Mechanical Properties Metric English Comments
Tensile Modulus 11.44 GPa
1659 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp EFP36G PEI
LNP* EFP36G is a Polyetherimide base resin containing a Mixed Glass Fiber and PTFE/Silicone.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 11.44 GPa
1659 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI
LNP THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing 30% Glass Fiber.