Polymer Property : Tensile Modulus = 11.08 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 11.08 GPa
1607 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP UX08325 PPA (Asia Pacific)
LNP* Thermocomp* UX08325 is PPA base glass fiber filled compounds, good for LDS (Laser direct structuring)application. Additional feature is high heat.