Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.02 GPa | 1598 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFL16 PA 66 LNP* LUBRICOMP* RFL16 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 11.02 GPa | 1598 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10 LNP* THERMOCOMP* QF0069 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Tensile Modulus | 11.02 GPa | 1598 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated, Easy Molding. |