Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.710 GPa | 103 ksi | ISO 527 |
Quadrant EPP Cestidur™ Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Tensile Modulus | 0.710 GPa | 103 ksi | MD; ASTM D882 |
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E.. |
|||
Tensile Modulus | 0.710 GPa | 103 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6 LNP* Thermocomp* PH0600B is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC.. |
|||
Tensile Modulus | 0.710 GPa | 103 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6 (Asia Pacific) LNP* Thermocomp* PH0600B is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC.. |
|||
Tensile Modulus | 0.710 GPa | 103 ksi | ISO 527-1/-2 |
Unitika EX-1222 PA6, Conditioned High-impact nylonInformation provided by Unitika Ltd. |