Mechanical Properties Metric English Comments
Tensile Modulus 10.95 GPa
1588 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DEL339XF PC
LNP* STAT-KON* DEL339XF is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Flame Retardant, Wear Resistant.
Tensile Modulus 10.95 GPa
1588 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DEL339XF PC (Asia Pacific)
LNP* Stat-kon* DEL339XF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant,..