Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.88 GPa | 1578 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFL46ES PA 66 LNP* LUBRICOMP* RFL46ES is a compound based on Nylon 6/6 containing 30% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Heat Stabilized, Easy Molding. |
|||
Tensile Modulus | 10.88 GPa | 1578 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC (Asia Pacific) LNP* Thermocomp* DF004P is a Polycarbonate base resin containing Glass Fiber. Characteristics of this grade are Exceptional Processing. |
|||
Tensile Modulus | 10.88 GPa | 1578 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP UX08325 PPA (Asia Pacific) LNP* Thermocomp* UX08325 is PPA base glass fiber filled compounds, good for LDS (Laser direct structuring)application. Additional feature is high heat. |