Tensile Modulus 10.47 GPa
1519 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp WC003P Polyester Elastomer
LNP* Thermocomp* WC003P is a compound based on Polyester resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A..