Polymer Property : Tensile Modulus = 10.22 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 10.22 GPa
1482 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp WX01910L PBT
LNP* Thermocomp* WX01910L is a compound based on Thermoplastic Polyester containing Proprietary Fillers. Characteristics of this grade are: Low Extractable.This data was supplied by SABIC-IP for t..