Mechanical Properties Metric English Comments
Tensile Modulus 10.21 GPa
1481 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Ultem ATX203R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 10.21 GPa
1481 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 10.21 GPa
1481 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Tensile Modulus 10.21 GPa
1481 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RX96592 PA 66
LNP* Thermocomp* RX96592 is a compound based on Nylon 6/6 containing Proprietary Fillers.
Tensile Modulus 10.21 GPa
1481 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON RE0029 PA 66
LNP* STAT-KON* RE0029 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.