Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.051 GPa | 1457.8 ksi | ISO 527 Type 1A |
Solvay TECHNYL® AR 218 V33 Black 34 N Nylon 66, 33% glass fiber, DRY Description: Polyamide 66, reinforced with 33% of glass fiber, containing recycled material, for injection molding, specially stabilized to improve its resistance to automotive cooling liquids.Avail.. |