Polymer Property : Tensile Modulus = 10.05 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 10.05 GPa
1458 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66
LNP* LUBRICOMP* RFL36L is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
Tensile Modulus 10.05 GPa
1458 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 (Asia Pacific)
LNP* Lubricomp* RFL36L is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.