Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.7327 GPa | 251.31 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LH-0300 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.7327 GPa | 251.31 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LH-0300 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |