Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.585 GPa | 229.9 ksi | ASTM D638 |
Eastman Tritan LX201 Copolyester Eastman Tritan LX201 is an amorphous copolyester with excellent appearance and clarity. Tritan LX201 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Tensile Modulus | 1.585 GPa | 229.9 ksi | ASTM D638 |
Eastman Tritan MX810 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceOutstanding impact re.. |
|||
Tensile Modulus | 1.585 GPa | 229.9 ksi | ASTM D638 |
Eastman Tritan MX811 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceGood heat resistanceO.. |
|||
Tensile Modulus | 1.585 GPa | 229.9 ksi | ASTM D638 |
Eastman Tritan TX2000 Copolyester Eastman Tritan TX2000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc.. |
|||
Tensile Modulus | 1.585 GPa | 229.9 ksi | ASTM D638 |
Eastman Tritan TX2001 Copolyester Eastman Tritan TX2001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX2001 contains a mold release derived from vegetable based sources. Its most outstanding fe.. |