Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0103 GPa | 1.50 ksi | ASTM D1708 |
DuPont Elvax® 4260 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 4260 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications. Applications:Elvax® 4260 resins can be used for the following applications: adhesives,.. |