Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.447 GPa | 209.9 ksi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers Centrex® 485 Sheet Extrusion Grade Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it.. |