Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.300 GPa | 188.5 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437C30L Calcium Reinforced |
|||
Tensile Modulus | 1.300 GPa | 188.5 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437T20L1 Talc Reinforced |
|||
Tensile Modulus | 1.300 GPa | 188.5 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437W20L Wollastonite Reinforced |
|||
Tensile Modulus | 1.300 GPa | 188.5 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336C10L1 Calcium Reinforced |
|||
Tensile Modulus | 1.300 GPa | 188.5 ksi | ASTM D638 |
Aclo Accucomp Polypropylene HPO306L Homopolymer |
|||
Tensile Modulus | 1.300 GPa | 188.5 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0436C20L1 Calcium Reinforced |
|||
Tensile Modulus | 1.300 GPa | 188.5 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0436T10L Talc Reinforced |