Polymer Property : Tensile Modulus = 1.29 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.29 GPa
187 ksi
1 mm/min
Arkema Group Rilsan® BMF Nylon 11 (Conditioned)
Designation ISO 1874-PA11,M,12-010Rigid grade for injection molding. Available color: natural. Additive free.Good melt viscosity. Outstanding ability to mold part with high length-thickness ratio an..