Mechanical Properties Metric English Comments
Tensile Modulus 0.903 GPa
131 ksi
X, Y-Direction; ASTM D638
Rogers Corporation RO3003 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Features and Benefits: