Polymer Property : Tensile Modulus = 0.885 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.00610 GPa
0.885 ksi
ISO 527-2
Solvay Specialty Polymers Polidan® EC/51 Polyethylene, Crosslinked (XLPE)
Flexible low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards com..