Tensile Modulus | 0.00552 GPa | 0.801 ksi | Type IV, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3904 Polyvinyl Chloride, Flexible (PVC, Flexible) A Clear-Frosted PVC compound formulated specifically for FDA extrusion and Molding applications.The physical properties listed below, are typical values obtained on compression molded sheets and tes.. |
|||
Tensile Modulus | 0.00552 GPa | 0.801 ksi | Method A, 20 in/min; ASTM D412 |
PolyOne Geon™ Vinyl Flexible XV 1197 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Modulus | 0.00552 GPa | 0.801 ksi | Type IV, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3902 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |