Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.740 GPa | 107 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Nemcon™ E - PP AS Polypropylene, Anti-Static Nemcon™ E-Series products are designed for use in ESDA electronic assembly environments. E PP AS is a moisture independent anti-static polypropylene characterized by consistent moldability and recy.. |