Polymer Property : Tensile Modulus = 0.621 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.345 - 0.621 GPa
50.0 - 90.0 ksi
ASTM D638
Arkema Group Kynar Flex® 2950 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Tensile Modulus 0.483 - 0.621 GPa
70.0 - 90.0 ksi
ITW Plexus Plexusâ„¢ MA422 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, medium open time.Information provided by Illinois Tool Works.
Tensile Modulus 0.483 - 0.621 GPa
70.0 - 90.0 ksi
ITW Plexus Plexus™ MA922 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, medium open time.Information provided by Illinois Tool Works.