Polymer Property : Tensile Modulus = 0.621 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.621 - 0.758 GPa
90.0 - 110 ksi
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois ..
Tensile Modulus 0.621 GPa
90.0 ksi
ASTM D638
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol
Tensile Modulus 0.621 GPa
90.0 ksi
ASTM D638
Ecomass® 4703ZD84 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technica..
Tensile Modulus >= 0.621 GPa
>= 90.0 ksi
5% strain; ASTM D790
BCC Products BC 8782 Urethane Casting
BC 8782 produces a high impact rigid 82 Shore D material that is commonly used to make clear or tinted castings of all kinds. When used at room temperature castings 1/8" thick or larger can be readi..
Tensile Modulus 0.621 GPa
90.0 ksi
TM R050-36
Resinlab® EP1305LV Black Epoxy Casting Resin
Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c..
Tensile Modulus 0.621 GPa
90.0 ksi
TM R050-36
Resinlab® EP1305LV Clear Epoxy Casting Resin
Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c..