Polymer Property : Tensile Modulus = 0.283 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.283 GPa
41.0 ksi
ISO 527
Lubrizol ESTANE® GP72DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 72DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, TranslucentAvailable in EuropeInformati..