Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.279 GPa | 40.5 ksi | TD |
Kuraray HYBRAR® BF1 Three Layer Blown Film Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber w.. |