Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.270 GPa | 39.2 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers |