Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.00150 GPa | 0.217 ksi | ASTM D412 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2350 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |
|||
Tensile Modulus | 0.00150 GPa | 0.217 ksi | ASTM D412 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2375 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |