Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.14584 GPa | 21.153 ksi | Storage |
Epoxy Technology EPO-TEK® H20F Electrically Conductive, Flexible Epoxy Product Description: EPO-TEK® H20F is a two component, flexible silver epoxy. It was designed for flexible type circuitry, such as switching circuits in a flexible panel system, as well as large di.. |